Film sticking, melt residue, and wear on a packaging machine may not originate from the same part. Heat-sealing jaws, heating bars, cutters, and transfer surfaces perform different tasks. Preparing a coating request starts with identifying the contact point where the problem occurs.

From system type to part function

System names such as flow-pack, vacuum, or shrink provide general context, but they are not enough to select a coating. Describe the film, contact temperature, and machine arrangement as well. A surface that reduces film sticking does not, on its own, guarantee package seal integrity. Settings such as pressure, alignment, and contact time require separate assessment.

For cutters, examine the cutting edge and mounting dimensions; for transfer surfaces, examine friction and wear. Do not assume that every surface will be coated. Drawings should identify holes, connections, and dimensional areas that must be protected. Address the effect of coating thickness on machine fit at the outset.

Temperature information for heated parts

The control panel setting should not be treated as the bar or jaw surface temperature. Report heating during idle periods and short-term peak conditions. Assess the selected system’s limits using its technical data. A high-temperature or ceramic designation does not establish suitability for every film.

  • Machine, part function, and technical drawing
  • Film or packaging material
  • Temperature, pressure, and contact time
  • Areas where residue or damage occurs
  • Cleaning chemicals and tools used

Evaluate the trial through the package

Discussions with Powerpan should define preparation, stripping, and the scope of the new surface application. Run the trial with the actual film and machine conditions. Continue the plant’s package acceptance checks alongside monitoring film release, residue buildup, and surface integrity.

Alignment or pressure may change when the machine is reassembled. These differences should not be confused with the effect of the coating. If the problem occurs only with a particular film, include it in the trial scope. One satisfactory package does not establish results for every operating setting.

Hard scraping during maintenance can damage the coating. If peeling or blistering occurs, remove the affected part from use for technical inspection. Confirm delivery time and spare-part planning according to the actual application scope. Do not assume that parts of any size can be processed or that refurbishment can be completed without downtime.

Record the settings and cleaning method used when changing films. Residue left by different films on the same jaw should not be interpreted as a single general surface problem. Including these changes in the trial clarifies the conditions under which the new coating was assessed and the uses to which the results apply.

Contact us for a project quotation

Tell us about your baking equipment or recoating requirements, including dimensions, quantities and operating conditions.