Tray Teflon coating is a PTFE-based application considered for making product release easier on industrial baking surfaces. A flat cookie tray and a perforated oven tray do not have the same geometry. Coating selection should consider material and operating conditions, not simply the tray’s name.

Powerpan’s assessment considers the product being baked, oven program, and existing cleaning method. Surface contact during baking, cooling, and stacking also matters. Nonstick coating does not automatically correct tray bending, oven settings, or a problem in the product recipe.

Preserving openings in perforated trays

On a perforated surface, holes, hole edges, and the metal areas in contact with the product are examined together. The openings must retain their function after application; layer buildup must not adversely affect the geometry. The intended use related to airflow is assessed using the tray drawing and existing construction.

For rimmed trays, base-to-wall transitions and stacking points are checked separately. On large flat surfaces, distortion and impact marks matter. Bodies showing cracks, corrosion, or surface loss after the old coating is stripped require a separate suitability decision.

Information for system selection

  • Tray material, dimensions, and surface type.
  • The product being baked and release agent used.
  • Oven program and conditions in which empty trays are held.
  • Cleaning chemicals and stacking method.

Food-contact scope is assessed through the relevant system’s documentation. General PTFE temperature values should not be applied to every tray coating. The applied system’s technical information and actual surface conditions must be considered together. Open flames or unusual heat exposure must be identified separately.

During initial use, product release can be observed in different areas of the tray. If marks, residue, or tearing appear on the product base, their location is recorded. Performing this check with the same recipe and program allows a better comparison of application results.

Do not use tools that cut or scrape the surface during cleaning, and reduce rubbing between coated areas during stacking. Trays with delamination should be removed from production and submitted for a quality assessment. For bulk renewal, tray types and damage conditions should be grouped separately; the delivery plan should be confirmed after inspection.

Contact us for a project quotation

Tell us about your baking equipment or recoating requirements, including dimensions, quantities and operating conditions.